Silicon dioxide to silicon etch selectivity in reactive ion etching (RIE) employing fluorocarbon gases is due to the formation of a fluorocarbon film on the substrate. This implies that etch selectivity is not achieved instantly but that the substrate will exhibit a transient etch rate and hence material loss during the film formation period. The amount of silicon lost during overetching for CF4/H2 RIE was determined by Rutherford backscattering spectrometry employing a buried marker. For standard etching conditions, about 7 nm of silicon is lost within the first minute of overetching as compared to 1.5 nm expected from steady-state etch rate data. The Si etch rate varies strongly as a function of time and decreases by a factor of greater than 10 within the first 30 s of overetching to approach a steady-state value.
A.D. Marwick, G.S. Oehrlein, et al.
Physical Review B
M. Haverlag, D. Vender, et al.
Applied Physics Letters
A. Henry, O.O. Awadelkarim, et al.
Materials Science and Engineering B
G.S. Oehrlein, R.M. Tromp, et al.
JES