About cookies on this site Our websites require some cookies to function properly (required). In addition, other cookies may be used with your consent to analyze site usage, improve the user experience and for advertising. For more information, please review your options. By visiting our website, you agree to our processing of information as described in IBM’sprivacy statement. To provide a smooth navigation, your cookie preferences will be shared across the IBM web domains listed here.
Conference paper
Preparation and in-situ surface analysis of MNFE/NIFE exchange structures: interfacial impurity incorporation
Abstract
MnFe/NiFe exchange structures have been prepared in an ultra-high vacuum sputtering/surface analysis system. Controlled introduction of residual gas impurities such as O2 and H2O at the MnFe/NiFe interface is studied by in-situ x-ray photoelectron spectroscopy (XPS) and the exchange structures are magnetically characterized. Due to the extreme reactivity of the NiFe surface towards O2 the exchange coupling is severely degraded by only small exposures of this molecule to the NiFe surface. In contrast, H2O does not oxidize the NiFe surface and therefore can be tolerated in greater quantities in the sputtering chamber without detrimental loss of exchange. This understanding of the basic surface chemistry of the MnFe and NiFe surfaces can lead to improved sputtering practices in actual manufacturing applications.