About cookies on this site Our websites require some cookies to function properly (required). In addition, other cookies may be used with your consent to analyze site usage, improve the user experience and for advertising. For more information, please review your options. By visiting our website, you agree to our processing of information as described in IBM’sprivacy statement. To provide a smooth navigation, your cookie preferences will be shared across the IBM web domains listed here.
Paper
Uniform Growth of Sub-5-Nanometer High-κ Dielectrics on MoS2 Using Plasma-Enhanced Atomic Layer Deposition
Abstract
Regardless of the application, MoS2 requires encapsulation or passivation with a high-quality dielectric, whether as an integral aspect of the device (as with top-gated field-effect transistors (FETs)) or for protection from ambient conditions. However, the chemically inert surface of MoS2 prevents uniform growth of a dielectric film using atomic layer deposition (ALD) - the most controlled synthesis technique. In this work, we show that a plasma-enhanced ALD (PEALD) process, compared to traditional thermal ALD, substantially improves nucleation on MoS2 without hampering its electrical performance, and enables uniform growth of high-κ dielectrics to sub-5 nm thicknesses. Substrate-gated MoS2 FETs were studied before/after ALD and PEALD of Al2O3 and HfO2, indicating the impact of various growth conditions on MoS2 properties, with PEALD of HfO2 proving to be most favorable. Top-gated FETs with high-κ films as thin as ∼3.5 nm yielded robust performance with low leakage current and strong gate control. Mechanisms for the dramatic nucleation improvement and impact of PEALD on the MoS2 crystal structure were explored by X-ray photoelectron spectroscopy (XPS). In addition to providing a detailed analysis of the benefits of PEALD versus ALD on MoS2, this work reveals a straightforward approach for realizing ultrathin films of device-quality high-κ dielectrics on 2D crystals without the use of additional nucleation layers or damage to the electrical performance.