Ann-Kathrin Michel, Anna Corinna Niemann, et al.
Journal of Physics D: Applied Physics
Nickel-rich NiFe thin films (Ni92Fe8, Ni89Fe11 and Ni83Fe17) were prepared by combining atomic layer deposition (ALD) with a subsequent thermal reduction process. In order to obtain Ni x Fe1-xO y films, one ALD supercycle was performed according to the following sequence: m NiCp2/O3, with m = 1, 2 or 3, followed by one FeCp2/O3 cycle. The supercycle was repeated n times. The thermal reduction process in hydrogen atmosphere was investigated by in situ x-ray diffraction studies as a function of temperature. The metallic nickel iron alloy thin films were investigated and characterized with respect to crystallinity, morphology, resistivity, and magnetism. As proof-of-concept magnetic properties of an array of Ni83Fe17, close to the perfect Permalloy stoichiometry, nanotubes and an isolated tube were investigated.
Ann-Kathrin Michel, Anna Corinna Niemann, et al.
Journal of Physics D: Applied Physics
Siegfried Karg, Vanessa Schaller, et al.
ESSDERC 2016
Johannes Gooth, Mattias Borg, et al.
Nano Letters
Johannes Gooth, Vanessa Schaller, et al.
Applied Physics Letters