About cookies on this site Our websites require some cookies to function properly (required). In addition, other cookies may be used with your consent to analyze site usage, improve the user experience and for advertising. For more information, please review your options. By visiting our website, you agree to our processing of information as described in IBM’sprivacy statement. To provide a smooth navigation, your cookie preferences will be shared across the IBM web domains listed here.
Publication
IITC 2000
Conference paper
A high performance 0.13 μm copper BEOL technology with low-k dielectric
Abstract
The integration of dual damascene copper with low-k dielectric at the 0.13 μm technology node is described. Up to five levels of copper wiring at three different metal pitches is provided in a spin-on organic inter metal dielectric (SiLK™ semiconductor dielectric. The Dow Chemical Co.). Additional global wiring levels in fluorosilicate glass (FSG) at two different relaxed metal pitches result in a total of up to eight levels of hierarchical wiring for enhanced BEOL performance. Successful integration was achieved while maintaining reliability standards. Development of new advanced unit processes was required to meet the challenges presented by this work. Patterning and passivation methodologies are discussed. A key feature of the integration scheme and material set reported is the resulting reduction in complexity compared to other proposed low-k integration alternatives for the current generation.